PC Injection Cycle Fluctuation—Drying Fluctuation
문제 현상
The same batch of material is normal in the morning but silver streaks appear in the afternoon, with no process change.
원인 분석
Dryer dew point drift, hopper insulation failure, or ambient humidity changes cause the dried PC to re-absorb moisture; PC absorbs moisture fast, and exposure for 1~2 hours may exceed the standard.
해결 방법
①Monitor the dryer dew point and regularly regenerate the molecular sieve; ②Seal the drying hopper and maintain insulation; ③Shorten the exposure time after drying; ④Strengthen verification in humid seasons.
핵심 요약
PC drying's enemy is 'secondary moisture absorption'.