Material Drying 4 조회수

PCABS hopper heat preservation 80℃

문제 현상
【Problem Phenomenon】Qualified dried PC/ABS regains moisture in the hopper, silver streaks recur in afternoon parts
원인 분석
Dried material in an open hopper regains moisture beyond the standard in 2-3 hours; a heat-preservation hopper maintaining 80℃ can delay moisture regain and is a necessary configuration for continuous production; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
해결 방법
Hopper heat preservation at 80℃ with cover; batch feeding to control residence ≤2h; direct connection of hopper dryer in humid seasons; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
PC/ABS hopper heat preservation 80℃, 2 hours residence is the moisture regain warning line; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
hopper heat preservationmoisture regain80℃residence

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다

ChemAI