PCABS Shear Silver Streaks
문제 현상
[Problem Phenomenon] PC/ABS silver streaks consistently appear near the gate or in high-speed filling areas
원인 분석
Shear overheating type silver streaks: excessive injection speed and too small gate cause local friction heat generation, cracking and gas production; the location is fixed in the shear concentration area; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Reduce injection speed and change to multi-stage; enlarge gate size; appropriately lower melt temperature in shear areas; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
핵심 요약
Shear silver streaks are fixed near the gate; reduce speed and enlarge the gate; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!