Injection Molding 6 조회수

PC injection pressure 100-150MPa

문제 현상
Thin-walled parts underfilled with short shots, or flash, mold expansion, and demolding difficulty
원인 분석
PC melt viscosity is high, requiring higher injection pressure to drive filling; thin-walled long-flow parts need 120-145MPa; but excessive pressure will expand the mold producing flash and greatly increase residual stress
해결 방법
①Injection pressure set at 100-150MPa adjusted according to wall thickness and flow length; ②Holding pressure takes 50-75% of injection pressure; ③Cooperate with multi-stage speed control to reduce end pressure
핵심 요약
PC's high viscosity determines high pressure demand; pressure just sufficient is enough, excessive pressure brings stress and flash, requiring fine grading according to structure;After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PC;injection pressure;100-150MPa;holding pressure;multi-stage injection