Material Drying 7 조회수

PC drying temperature 120℃ upper limit

문제 현상
【Problem Phenomenon】Raising drying temperature for speed, PC pellets instead agglomerate and discolor
원인 분석
PC drying temperature 120℃ is appropriate; above 120℃ pellets soften and stick and thermally oxidize and discolor; temperature and time must be balanced, not the higher the faster;During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
해결 방법
Drying temperature controlled at 110-120℃; time 3-4h; agglomerated material screened out, discolored material downgraded;After adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
PC drying 120℃ is the upper limit, agglomeration and discoloration are overtemperature signals;After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence;Include this case in the defect archive as a reference for troubleshooting similar problems in the future