Yellowing and Black Specks in PE Injection Molded Products

문제 현상
Natural-color PE parts turn yellow, or light-colored parts show black specks and black streaks, resulting in poor appearance.
원인 분석
Excessive melt temperature or too long residence time causes thermal degradation yellowing; material accumulated in dead spots of the barrel/hot runner carbonizes and falls off to form black specks; regrind contamination and high-temperature idling with heat preservation also introduce them.
해결 방법
①Lower the melt temperature to a reasonable range and shorten residence time; ②Thoroughly purge the machine and disassemble and clean dead spots; ③Avoid prolonged high-temperature idling of the barrel; ④Check the cleanliness of raw material and regrind; ⑤Evaluate whether the antioxidant system matches.
핵심 요약
PE yellowing and black specks = 'excessive heat history + dead spot carbonization': lower temperature and shorten time to prevent yellowing, purge the machine and check material to prevent black specks; for intermittent black specks, focus on checking equipment dead spots instead of repeatedly fiddling with the process.
PE;yellowing;black speck;thermal degradation;carbonization;dead spot

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다

ChemAI