Molds & Tooling 3 조회수

Thermal Expansion Out of Control of PEEK High-Temperature Molds

문제 현상
PEEK molds show guide pin seizure, slide galling, and fitting surface scoring at working temperatures of 180~200℃, and mold life is significantly shortened.
원인 분석
When the mold rises from room temperature to the high-temperature working zone, the thermal expansion of each component differs; fits designed at room temperature become interference-stuck at high temperature; long-term high-temperature operation of PEEK molds accelerates wear of guide components.
해결 방법
①Design the mold fitting clearances corrected for the thermal expansion at working temperature; ②Select high-temperature-resistant mold steel and high-temperature lubrication; ③Preheat the mold and heat up slowly to reduce thermal shock; ④Establish a special maintenance cycle for high-temperature molds.
핵심 요약
PEEK mold design must consider the thermal expansion at 200℃-level working temperatures; room-temperature fitting data cannot be directly applied; the maintenance cost of high-temperature molds should be included in the project budget.
PEEK;mold;thermal expansion;high temperature;seizure;wear