Molds & Tooling 3 조회수

Excessive Post-Shrinkage of PEEK Products

문제 현상
PEEK products are dimensionally qualified at demolding, but dimensions continue to change after several days of storage or high-temperature use, and fits go out of tolerance during assembly, causing complaints.
원인 분석
Insufficiently crystallized amorphous regions undergo secondary crystallization upon subsequent heating, accompanied by volume shrinkage; slow relaxation of internal stress also causes slight shape change; the high-temperature use environment accelerates the post-shrinkage process.
해결 방법
①Raise the mold temperature to ensure crystallization is fully completed during molding; ②Subject products to temperature-conditioning setting treatment; ③Reserve post-shrinkage compensation in mold design; ④Perform dimensional aging verification at the use temperature.
핵심 요약
The root of PEEK post-shrinkage is still crystallinity management; completing crystallization properly during molding is the most thorough solution; high-temperature applications must undergo aging dimensional verification before finalizing the design.
PEEK;post-shrinkage;secondary crystallization;aging;dimensions;setting