Regrind Proportion of PEEK Exceeding the Limit

문제 현상
[Problem Phenomenon] The quality of PEEK products blended with regrind declines, and the problem is more prominent for filled grades
원인 분석
Regrind increases heat history and cross-contamination risk, and high-temperature processing amplifies the influence of trace impurities; Victrex specifies regrind upper limits: 30% for virgin material, 10% for filled grades
해결 방법
Limit regrind to within 30% for virgin material and within 10% for filled material, dried separately; grind and sieve regrind to prevent foreign matter; prohibit regrind for critical performance parts; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
PEEK regrind limits of 30% for virgin and 10% for filled are the official red line — exceeding them plants hidden dangers; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence