Molds & Tooling 3 조회수

Insufficient Runner and Gate Dimensions for PEEK

문제 현상
[Problem Phenomenon] PEEK has large flow resistance and is difficult to fill, with pressure loss concentrated in the runner and gate
원인 분석
PEEK's high viscosity requires medium runners and large gates: Victrex 150G recommends runner/nozzle diameter >3mm, sub-runner >3.5mm, gate >1mm or 0.5 times the wall thickness; too-small dimensions cause large pressure loss and shear degradation
해결 방법
Enlarge runner and gate dimensions according to the data sheet lower limits; enlarge further for high-viscosity grades; when a too-small gate causes shear problems, prioritize enlarging the gate rather than raising temperature; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
Runner >3mm and gate >1mm for PEEK are the official lower limits — when pressure loss is large, measure the dimensions first; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
runner size gate size pressure loss shear