Molds & Tooling 3 조회수

PEI Excessively Fast Freezing and Insufficient Filling

문제 현상
PEI products have incomplete filling in thin-walled and long-flow areas; raising the melt temperature to fill the cavity instead causes degradation, and the process falls into a dilemma.
원인 분석
PEI molding has a unique characteristic: the product freezes particularly fast; the melt front freezes quickly causing short shots; precisely because of fast freezing, PEI products rarely show obvious sink marks, but the filling window is extremely narrow.
해결 방법
①Increase the mold temperature (140~180℃) to make the product freeze slowly; ②improve the mold runner to ensure fast and uniform melt injection; ③injection speed at 50~80% of the screw's maximum speed; ④coordinate with a larger runner design.
핵심 요약
PEI's fast freezing is a double-edged sword of the material: free of sink marks but difficult to fill; high mold temperature and fast injection are the correct countermeasures; raising melt temperature is the wrong path.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PEI;fast freezing;filling;mold temperature;runner;short shot

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다