PEI Clamping Force Configuration
문제 현상
PEI production has flash and mold swelling problems; clamping force configured by experience is insufficient, and glass fiber reinforced grades require more.
원인 분석
PEI clamping force needs to provide 4~6 tons per square inch of projected area; glass fiber reinforced resins may require higher clamping force; high injection pressure processes impose rigid constraints on clamping requirements.
해결 방법
①Calculate clamping force at 4~6 tons per square inch of projected area; ②appropriately increase for glass fiber reinforced grades; ③review the clamping margin for high-pressure processes; ④stop the machine immediately for inspection if mold swelling signs appear.
핵심 요약
PEI clamping force of 4~6 tons per square inch is a precise standard; increasing for reinforced grades is a detail; reviewing the clamping margin prevents equipment damage.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!