Material Drying
4 조회수
PEI Drying Equipment Requirements
문제 현상
After PEI is processed with ordinary drying equipment, the moisture still exceeds the standard; drying efficiency is low and drying quality is unstable between batches.
원인 분석
PEI recommends using a closed dehumidifying hot-air circulating hopper dryer with an aftercooler; the air dew point at the hopper inlet should be between -29℃ and -40℃ or lower; the equipment grade directly determines the drying effect.
해결 방법
①Configure a closed dehumidifying dryer with an aftercooler; ②verify the dew point at -29~-40℃ or lower; ③execute drying temperature and time according to the grade; ④regularly test the dew point and equipment performance.
핵심 요약
The dew point indicator of PEI drying equipment is a hard constraint; the closed design with aftercooler is the standard configuration; equipment performance is verified regularly.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다