Material Analysis 11 조회수

PEI Aviation Interior Part Flame Retardancy

문제 현상
PEI aviation interior parts have batch fluctuations in flame retardancy tests; although naturally flame retardant, product quality affects performance.
원인 분석
PEI has excellent natural flame retardancy, with an oxygen index of 47% and UL94 V-0 without adding flame retardants; but internal product defects such as bubbles affect flame retardant performance; thin-wall and thick-wall differences; processing degradation reduces performance.
해결 방법
①Non-destructive testing of product internal quality; ②control processing heat history; ③uniform wall thickness design; ④batch verification of flame retardant performance.; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
PEI's natural flame retardancy is a material advantage; product quality determines the realization of the advantage; batch verification ensures aviation safety.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PEI;aviation;flame retardancy;V-0;bubble;verification