Injection Molding 6 조회수

PESU Two-Color '2079851475616104452

문제 현상
PESU two-color or overmolding, interface bonding and process matching.
원인 분석
PESU two-color '2079851475616104452; material compatibility; temperature matching; interface strength; process window.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
해결 방법
①Compatibility verification; ②temperature matching; ③interface design; ④strength testing; ⑤process optimization.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
PESU two-color is a complex process; compatibility and matching are the foundation; testing ensures quality.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PESU; two-color; overmolding; interface; compatibility; temperature