Material Drying
7 조회수
PET Bottle Drop Rupture
문제 현상
Finished bottles crack at the bottom or body in drop tests, occasional bottle rupture and leakage during transportation, and the customer complaint rate increases.
원인 분석
Improper bottom wall thickness stretch distribution forms weak zones, or PET becomes brittle due to high-temperature degradation and insufficient-drying hydrolysis; stress concentration at the bottle bottom corners also induces drop rupture.
해결 방법
①Optimize bottom stretch ratio and material distribution; ②strengthen raw '2079851475616104451 before preform injection; ③reduce processing temperature to reduce degradation; ④test bottle bottom thickness and IV value.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
Drop performance is directly related to material toughness and wall thickness distribution; hydrolysis embrittlement and bottom weakness are the two major root causes, which need to be solved synergistically from drying, temperature and stretching process.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!