Extrusion & Post 4 조회수

PET preform inventory aging and hardening

문제 현상
Under the same process, old-batch preforms are difficult to stretch and prone to whitening during bottle blowing, and normal operation is restored after switching to a new batch of preforms.
원인 분석
After long-term storage, the IV of preforms slowly declines and the material hardens, requiring higher temperature to stretch; aged preforms stored for more than 6~12 months have a significantly narrowed process window.
해결 방법
①Check the production date of preforms and apply first-in-first-out; ②appropriately increase the heating temperature by 2~3% as compensation for aged preforms; ③control the inventory cycle; ④perform sampling tests of stretch performance on old preforms.
핵심 요약
Preforms have a shelf life concept, and aged preforms require process compensation; inventory management and batch traceability are the basic guarantees for stable bottle blowing quality.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PET;preform;aging;inventory;IV;shelf life