PET hot runner temperature
문제 현상
Stringing and crystallized white spots repeatedly appear at the gate of the preform hot runner
원인 분석
The hot runner temperature is uneven; when the gate zone temperature is low, the melt crystallizes prematurely, and when it is high, stringing and degradation occur; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Calibrate each hot runner temperature point to ±3℃; the gate area is independently temperature-controlled; lower the hot runner temperature during shutdown to prevent retained-material crystallization; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
The temperature control accuracy of the preform hot runner directly determines the gate quality; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!