PET preform uneven wall thickness

문제 현상
The preform wall thickness variation rate is too large; the blown bottles have uneven thickness and fail the pressure test
원인 분석
Excessive screw temperature or excessive back pressure changes the melt state; improper holding position and pressure cause uneven filling density; too low mold cooling water temperature affects uniform solidification; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
① Appropriately lower the screw temperature; ② adjust back pressure to a reasonable range; ③ optimize holding pressure position and set cooling water temperature at 8-10℃; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
Preform wall thickness uniformity is a prerequisite for blowing quality; the three parameters of temperature, holding pressure, and water temperature are adjusted in linkage; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PET;preform;wall thickness;holding pressure;cooling water temperature