Material Drying
3 조회수
PET silver streak identification
문제 현상
Silver streaks appear on PET preforms and are still not eliminated after enhanced drying
원인 분석
Besides moisture, PET silver streaks may also be caused by shear heat degradation or mixed foreign material; different causes require opposite countermeasures; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Observe the air-shot strand: bubble-like indicates moisture, silky transparent indicates shear; check mixing and screw wear; for moisture silver streaks, strengthen drying again; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
Identify silver streaks before treating them to avoid ineffective drying; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!