Molds & Tooling
3 조회수
PMMA Product Weld Line Venting
문제 현상
Burning and bubbles coexist at weld lines; both are eliminated simultaneously after venting improvement.
원인 분석
Two melt streams converge and envelop air; without a venting channel, the gas is compressed, burnt and remains as bubbles; the confluence area is a key blind spot for venting.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based on experience alone.
해결 방법
①Open vent grooves in the confluence area; ②set overflow wells to guide trapped air out; ③adjust gate to change confluence position; ④reduce speed to assist venting.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
핵심 요약
Weld line trapped air shows both burning and bubbles; venting plus overflow wells is the standard solution.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!