PMMA Environmental Stress Crazing
문제 현상
Fine crazing appears on products in storage without external force; environmental investigation finds large temperature and humidity fluctuations.
원인 분석
Residual stress is slowly released under temperature and humidity cycling, producing a crazing network on the surface; products with high stress levels are more prone to it.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based on experience alone.
해결 방법
①Anneal to eliminate residual stress; ②control storage environment stability; ③avoid contact with solvent vapor; ④optimize process to lower the stress starting point.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
핵심 요약
Storage crazing is a delayed manifestation of residual stress; annealing and storage environment management are a preventive combination.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!