Molds & Tooling 3 조회수

PMMA Mold Temperature 40-80

문제 현상
PMMA products produced with 30℃ mold temperature have surface flow marks and large internal stress
원인 분석
Too-low mold temperature causes the melt front to quench, flow marks freeze and molecular orientation stress is large; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based on experience alone.; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
해결 방법
Raise mold temperature to 60-80℃; optical parts mold temperature above 70℃; appropriately raise for thick-wall parts; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
핵심 요약
PMMA mold temperature is a key variable of surface quality and internal stress; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.; include this case in the defect archive as a troubleshooting reference for similar future problems.
PMMA mold temperature flow mark internal stress