Molds & Tooling 3 조회수

POM product dimensions too small (post-shrinkage)

문제 현상
Measurement at demolding is acceptable, but after 24 hours the dimensions continue to shrink out of tolerance.
원인 분석
POM has high crystallinity (shrinkage can reach more than 2%), continues to crystallize and shrink after demolding, with obvious changes within 24 hours; measuring too early gives a false pass.
해결 방법
①Place products at constant temperature for 24 hours before inspection; ②compensate the mold for a shrinkage of about 2% or more and correct according to actual measurement; ③unify measurement aging; ④anneal for stabilization if necessary.
핵심 요약
POM dimensions = only the dimensions after 24 hours count.
POM;post-shrinkage;dimension;crystallization;measurement aging