Short shot caused by early POM gate freezing

문제 현상
Thick-walled products have severe sink marks due to insufficient holding pressure, and inspection found that the gate size is small and the freezing time is too early.
원인 분석
A small gate cross-section causes it to solidify before the thick zone of the product, so feeding cannot continue during the holding stage; POM crystallizes fast and freezes fast, making the small gate problem more prominent.;During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
①Enlarge the gate size to delay freezing; ②increase the mold temperature to extend gate open time; ③shorten the runner length; ④set the holding pressure according to the solidification time of the thick zone.;After adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
The gate freezing time determines the effective feeding window; POM should adopt a larger gate design, combined with mold temperature management for holding pressure efficiency.;After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
POM;gate;freezing;holding pressure;feeding;short shot