Material Drying
3 조회수
POM low water absorption drying specification
문제 현상
POM products have poor surface gloss, occasional silver streaks, and appearance parts fail to meet requirements
원인 분석
POM has a water absorption rate of only 0.2-0.5% and is a low water absorption material, so drying is usually unnecessary; but surface moisture from humid seasons or improper storage can still cause silver streaks and reduce surface gloss, so appearance parts need routine drying
해결 방법
①Routine drying at 80°C×2-4 hours or 110-120°C×3-5 hours; ②moisture-affected raw material must be dried before use; ③for high-gloss appearance parts, list drying as a fixed process step
핵심 요약
POM drying is icing on the cake rather than a lifeline; routine 80°C×2-4h, moisture-affected material must be baked, appearance parts have a fixed drying process; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!