POM drying temperature and time
문제 현상
After POM was dried at 120°C for 4 hours, the pellets turned yellow and molding produced a pungent odor
원인 분석
POM has limited thermal stability, and long-time drying at 120°C has already triggered thermo-oxidative degradation, releasing formaldehyde and breaking molecular chains; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Control POM drying at 80-100°C×2-3 hours, not exceeding 110°C; use as soon as possible after drying; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
POM drying is a gentle process, and over-temperature drying equals pre-degradation; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!