POM Pressure Sensitivity for Flow Adjustment
문제 현상
Raising barrel temperature to improve flowability is ineffective and instead causes degradation; the part is still underfilled
원인 분석
POM melt viscosity is insensitive to temperature and approximates a Newtonian fluid, so raising temperature has poor viscosity-reducing effect and approaches the decomposition temperature; it is sensitive to injection pressure changes, so flow adjustment should follow the pressure and speed route
해결 방법
①To improve flow, prioritize increasing injection pressure and speed; ②set temperature only according to the window baseline; ③if necessary, reduce nozzle size to increase shear; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
The correct means of adjusting POM flow is pressure, not temperature; the temperature-raising route is a typical wrong direction for POM; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!