Material Drying 3 조회수

Silver streaks on PP injection molded parts

문제 현상
Silvery-white streaks appear on the product surface along the flow direction, which diminish after drying.
원인 분석
Moisture adsorbed on the surface of PP pellets vaporizes in the melt; degradation gas or shear overheating can also produce similar silver streaks.; during on-site investigation, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
해결 방법
①Dry the pellets appropriately; ②control the melt temperature to prevent degradation; ③reduce the screw speed to reduce shear; ④check the moisture content and quality of the regrind.; after adjustment, continuously sample and verify the effect, and resume mass production after confirming stability
핵심 요약
Investigate PP silver streaks along the three clues of moisture, degradation, and shear; verify by drying first, then check the temperature history.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PP; silver streaks; moisture; degradation; shear; drying