Molds & Tooling 4 조회수

Trapped gas burning of PP products

문제 현상
Burnt marks appear at the end of the material flow, which are eliminated after venting improvement.
원인 분석
The venting at the end of the cavity is poor, and the air is adiabatically compressed and burns the melt; high-speed filling makes trapped gas more serious.; during on-site investigation, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
해결 방법
①Open vent grooves at the end; ②reduce the injection speed; ③clean the blocked vent grooves; ④optimize the gate position.; after adjustment, continuously sample and verify the effect, and resume mass production after confirming stability
핵심 요약
The location of trapped gas burning is the point to add venting; venting design for thin-wall high-speed parts should be considered in advance.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PP; trapped gas; burning; venting; end; injection speed