Molds & Tooling 5 조회수

PPO Conventional Mold Temperature Range Differences

문제 현상
【Problem Phenomenon】Different documents have mold temperature ranges of 60-100℃, 100-150℃, 71-104℃ coexisting, causing hesitation in setting
원인 분석
Mold temperature range differences stem from grades and goals: PX1181 is 60-100℃, recybase is 71-104℃, GTX974 is 100-150℃; low mold temperature benefits the cycle, high mold temperature improves flow, weld lines and surface
해결 방법
Set according to the grade data sheet range; appearance and weld line sensitive parts take the upper limit; cycle-priority parts run at the lower limit with quality verification; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
PPO mold temperature range varies by grade; take the upper limit for flow, surface and weld lines; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
mold temperature rangegradeweld linecycle