문제 현상
【Problem Phenomenon】Cold slugs or overheating at the PPO nozzle, and defects in the front section of products recur
원인 분석
Nozzle temperature is generally about 10℃ lower than barrel temperature (GTX974 data), while SABIC recommends nozzle and melt temperature in the same range of 280-300℃; improper setting causes cold slug blockage or local overheating
해결 방법
Start nozzle temperature 10℃ lower than barrel temperature and calibrate with actual measurement; for cold slug head problems, check nozzle heating and bore; for overheating, lower 5-10℃ and verify; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
PPO nozzle starts 10℃ lower than the barrel; for both cold slugs and overheating, check the measured temperature; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence