문제 현상
[Problem Phenomenon] Burning and blackening at the end ribs of PPO products, accompanied by odor
원인 분석
During fast injection with long runners, insufficient venting causes trapped gas to heat up by adiabatic compression and burn; PPO thermal decomposition also produces corrosive gas, aggravating the harm; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Ensure sufficient mold venting to cooperate with fast injection; add venting at end ribs; reduce the final-stage injection speed for burnt parts; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
PPO burning is a mismatch between fast injection and venting; venting is the premise of fast injection; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!