PPO Black Specks and Carbonization Contamination
문제 현상
[Problem Phenomenon] Black specks scattered on PPO products, recurring intermittently after cleaning
원인 분석
Discolored degraded material with residence exceeding 2 hours, carbonized peeling from barrel dead spots and regrind contamination are sources of black specks; the corrosiveness of decomposition gas accelerates the deterioration of dead-spot material; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Strictly enforce residence time management; regularly clean the barrel and hot runner to check dead spots; manage regrind cleanliness and screening; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
For PPO black specks first check residence-discolored material, then check dead spots and regrind; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!