문제 현상
[Problem Phenomenon] PPO products stick to the mold and are scratched, with large demolding force and difficult ejection
원인 분석
Large internal stress and strong shrink-fit force make demolding difficult; excessive holding pressure, insufficient cooling and insufficient draft angle aggravate it; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Reduce holding pressure and internal stress; check draft angle and cavity polishing; extend cooling to ensure demolding strength; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
For PPO mold sticking first reduce internal stress, then check draft, polishing and cooling; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!