PPS Draft Angle

문제 현상
Parts are scratched during demolding and show ejector whitening, deep-cavity parts deform, and the yield rate fluctuates
원인 분석
PPS has high rigidity and high brittleness, and cracks easily under demolding force; the draft angle is 0.25-1° according to depth; the ejection system needs large-area balance; polishing reduces demolding resistance
해결 방법
①Draft angle 0.25-1°; ②Ejector pins arranged in large-area balance; ③Cavity polishing to reduce scratching; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
PPS demolding must accommodate its brittleness; the three elements of draft angle, balanced ejection, and polishing are all indispensable; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence