Injection Molding
6 조회수
PP Burnt Mark at the End
문제 현상
PP burnt marks at the flow end, trapped air adiabatic compression, speed and venting adjustment.
원인 분석
PP burnt marks at the flow end; air trapped adiabatic compression high temperature; injection speed too fast; poor venting; end confluence area; recurrence after purging.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
해결 방법
①Reduce injection speed; ②improve venting; ③end venting; ④purging; ⑤recurrence monitoring.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
Speed and venting are the adjustment directions for PP burnt; the end is the key area; monitoring prevents recurrence.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!