Injection Molding
4 조회수
GPPS Product Short Shot
문제 현상
Thin-wall transparent parts are incompletely filled.
원인 분석
Injection pressure and speed are insufficient or temperature is low; PS solidifies quickly, and the front easily freezes under thin-wall long flow paths.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
해결 방법
①Increase injection pressure and speed; ②appropriately increase material temperature and mold temperature; ③enlarge runners and gates; ④improve venting.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
Short shot is investigated from three paths: pressure, temperature and runner; pay attention to the thermal stability boundary of PS when raising temperature.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다