Material Analysis 11 조회수

PSU Internal Stress Difficult to Eliminate

문제 현상
PSU products have large internal stress after molding; cracks appear during storage or use; stress marks are visible on transparent parts; solvent contact accelerates cracking.
원인 분석
PSU melt cools relatively quickly and molecular chains are rigid, making the internal stress generated during molding difficult to eliminate; high-viscosity melt orientation freezes; rapid cooling and excessive holding pressure aggravate stress accumulation.
해결 방법
①Increase mold temperature to 150~180°C to slow stress freezing; ②Apply moderate holding pressure to avoid over-compaction; ③Anneal after molding to release stress; ④Eliminate sharp corners in the structure.
핵심 요약
Internal stress management is the fate of rigid, fast-cooling materials like PSU; high mold temperature and annealing are the two pillars; stress cracking verification must simulate the actual environment.; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence
PSU; internal stress; cracking; annealing; mold temperature; rigidity