Molding Process
7 조회수
PTFE Warpage and Distortion
문제 현상
PTFE parts bend and distort after sintering or cooling, assembly misaligns, and alignment of critical mechanical systems fails.
원인 분석
Uneven heating or cooling during sintering generates thermal gradients; PTFE sintering shrinkage is 15~20% and differential shrinkage is aggravated at uneven wall thickness; uneven molding pressure generates stress concentration.
해결 방법
①Controlled uniform heating and slow gradual cooling; ②Mold design with consistent wall thickness to reduce differential shrinkage; ③Set stress relief structures or anneal after sintering; ④Uniform molding pressure.
핵심 요약
Thermal management and wall thickness design are equally important for PTFE warpage; 15~20% sintering shrinkage is the baseline data for process design; annealing is an effective post-treatment means.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!