PVC Burnt: Check Temperature First
문제 현상
Burnt black specks appeared on products; the operator adjusted the mold and speed first, and the problem recurred
원인 분석
PVC defect statistics show temperature-related defects account for 55-60%; the first check item for burnt black specks is always temperature and residence time, not mold or speed; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
해결 방법
①For burnt, first check melt temperature and residence time; ②second check shear factors—screw speed and gate; ③finally check venting and mold; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
PVC troubleshooting has a clear priority; temperature first, shear second, venting third—checking in order is most efficient; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!