PVDF '2079851475616104452 Jetting Marks

문제 현상
【Problem phenomenon】Low-viscosity PVDF jets into the cavity through a small gate, with obvious snake patterns and flow marks near the gate
원인 분석
The low-viscosity melt passes the gate at high speed without contacting the wall, forming jetting, and the front folds into patterns; ZetarMold lists jetting as a common defect and recommends enlarging the gate or using an overlap fan gate
해결 방법
Enlarge the gate size or change to an overlap fan gate to guide wall-contacting filling; reduce the initial injection speed out of the gate; arrange the gate facing the core to use impact for wall contact; After adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
Low-viscosity PVDF jetting is eradicated by gate design; speed reduction is only an aid; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; Include this case in the defect archive as a reference for troubleshooting similar problems in the future
jetting marksgate designlow viscosityflow marks