Injection Molding
5 조회수
PVDF '2079851475616104452 Warpage
문제 현상
【Problem phenomenon】PVDF sheets and thin-walled parts warp and twist after demolding, and assembly accuracy fails to meet requirements
원인 분석
Uneven mold temperature distribution, inconsistent cooling, and internal stress release jointly cause warpage; crystallinity differences in semi-crystalline materials amplify the warpage tendency; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
해결 방법
Balance mold temperature distribution and optimize cooling water channels; symmetric design of thick-walled ribs; anneal at 80-120℃ after molding to release internal stress; symmetric holding pressure in the process to reduce residual stress
핵심 요약
The main causes of PVDF warpage are uneven mold temperature and internal stress; annealing is the follow-up measure to stabilize dimensions; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!