Production & Quality 5 조회수

PVDF and PFA Selection Confusion

문제 현상
【Problem phenomenon】Misuse of PVDF in high-temperature or ultra-pure occasions causes deformation or contamination, and misuse of PFA in cost-sensitive occasions causes waste
원인 분석
PFA withstands 260℃ and has extremely high purity, suitable for semiconductor ultra-pure systems; PVDF withstands about 150℃ but has better rigidity, wear resistance, and cost, suitable for industrial corrosion-resistant pipelines; the positioning difference between the two is clear
해결 방법
Select material according to temperature and purity requirements: choose PFA for above 150℃ or semiconductor ultra-pure, and PVDF for industrial corrosion-resistant pressure-bearing below 150℃; conduct a full life cycle evaluation combining cost and performance
핵심 요약
PVDF and PFA are selected by the boundary of temperature and purity, and 150℃ is the key watershed; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
material selectionPFAsemiconductortemperature resistance