Material Drying
5 조회수
TPE Delamination (Moisture Type)
문제 현상
Batches with insufficient drying show delamination coexisting with silver streaks.
원인 분석
After the material absorbs moisture, water vaporizes during '2079851475616104452, separating melt layers; hygroscopic TPE or damp batches have high incidence.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
해결 방법
①Dry according to the supplier data sheet; ②control drying temperature, time and dew point; ③sealed storage; ④re-dry damp batches.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
Moisture-type delamination and silver streaks share the same source; drying verification is the first troubleshooting action.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!