Processing Machinery 4 조회수

TPE Melt Temperature 180-220℃

문제 현상
Low melt temperature causes insufficient filling, high temperature causes degradation and discoloration, and nozzle drooling
원인 분석
The TPE melt temperature window is 180-220℃, the SBS system takes the middle-lower limit and the SEBS system takes the middle-upper limit; exceeding 220℃ causes thermal decomposition producing low-molecular substances, making products sticky and discolored
해결 방법
①Adjust melt temperature at 180-220℃ according to the system; ②SBS system 180-200℃, SEBS system 200-220℃; ③Cool down immediately if exceeding 220℃
핵심 요약
The TPE temperature window is graded by system; SBS and SEBS have different temperature strategies and cannot be borrowed from each other; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence