Material Drying
5 조회수
TPE Drying Judgment
문제 현상
Drying is omitted because TPE is nominally low-hygroscopic, and bubbles appear in overmolded products
원인 분석
The TPE matrix has low water absorption, but polar grades and overmolding materials still absorb moisture; overmolding interface bubbles are mostly related to moisture; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
해결 방법
General TPE 80℃×2 hours; overmolding materials and TPU types must be dried; moisture content controlled at 0.1%; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
TPE drying is distinguished by grade type; overmolding material must be dried; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!