TPE Overmolding Temperature Matching
문제 현상
The hard plastic substrate deforms during TPE overmolding, or insufficient TPE temperature causes poor bonding
원인 분석
TPE overmolding temperature must match the hard plastic substrate: PC substrate TPE temperature 200-220℃, ABS substrate 180-200℃, PP substrate 160-180℃; insufficient temperature gives poor bonding, excessive temperature deforms the hard plastic
해결 방법
①Set the TPE temperature according to the hard plastic substrate; ②Preheat the hard plastic to improve bonding; ③Verify temperature matching by mold trial; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
TPE overmolding temperature is a function of the substrate; PC, ABS, and PP each have corresponding windows, and mold trial verification is a necessary step; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence