문제 현상
TPE transparent parts are cloudy and yellow, transparency does not meet the standard, and there is color difference between batches
원인 분석
TPE transparent parts require SEBS base material; SBS base material is not yellowing resistant; moisture and degradation affect transparency; color masterbatch carrier selection affects hue; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
해결 방법
①Choose SEBS-based TPE for transparent parts; ②Strictly dry to below 0.1%; ③Select the color masterbatch carrier by base material; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
The foundation of TPE transparent parts lies in SEBS; yellowing resistance and drying control are the guarantee of transparency; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!