Extrusion & Post
11 조회수
TPE extrusion die buildup
문제 현상
Deposits retained at the edge of the TPE extrusion die, lines appear on the product surface
원인 분석
Causes of TPE die buildup: material dampness, inherent material characteristics, excessive filling oil; deposits periodically fall off and enter the product forming defects; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
①fully dry the material; ②add external lubricant; ③apply Teflon coating on the die to prevent sticking; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
핵심 요약
TPE die buildup is a dual signal of drying and formulation; Teflon coating is an effective hardware countermeasure; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다